摘  要:某环保项目半地下水池平面尺寸超长,为减少混凝土收缩裂缝,设计单位按规范要求设置伸缩缝。在水池满水试验中发现侧墙伸缩缝处渗漏。该文分析伸缩缝漏水的原因,并针对性地给出修复方案。

关键词:混凝土收缩裂缝;伸缩缝;满水试验;橡胶止水带;修复施工

中图分类号:TD744       文献标志码:A           文章编号:2095-2945(2023)03-0144-05

Abstract: The plane size of the semi-underground pool of an environmental protection project is very long. In order to reduce the shrinkage cracks of concrete, the design team sets up expansion joints according to the requirements of the code. The leakage at the expansion joint of the side wall was found in the full water test of the pool. In this paper, the cause of expansion joint leakage is analyzed, and the repair method is given.

Keywords: concrete shrinkage crack; expansion joint; full water test; rubber water stop; repair construction

混凝土是以水泥为胶凝材料,砂石为骨料,与水按一定配合比组成的复合材料,必要时还可增加外加剂和矿物掺合料改善性能。(剩余5702字)